Induction Soldering Steel Class: Induction Soldering
Intro: Soldering Steel Objective To heat a special steel housing to 500(260) F(C) for a soldering applicationMaterial Steel housingSolder wire and fluxTemperature 500(260) 550(287.8) F(C)Frequency 200 kHzEquipment Power of 6kW, 150-400 kHz solid state induc…
Induction Soldering Steel Tube Class: Induction Soldering
Intro: Soldering Steel Tube Objective Heat a.125” (3.175mm) diameter stainless steel tube to a 1” diameter cylinder 1” (25.4mm) tall for a soldering applicationMaterial Stainless steel cylinder and tubeTemperature indicating paint Lead free solder preform…
Induction Soldering copper Class: Induction Soldering
Intro: Soldering copperObjective Heat copper tab until the solder reflows.Material Copper tab 0.25 X 0.25 inch square about 0.05 inches thick.Lead free solder material (higher melting temperature than regular solder.)Temperature 500 F for 1.25 secondsFrequen…
Induction Shrink Fit Cast Iron Class: Induction Shrink Fitting
Intro: Shrink Fit Cast Iron Objective To use induction to prepare cast iron assemblies for shrink fit assemblyMaterial Customer supplied cast iron rocker arms of varying sizesTemperature 450 F (232 C)Process Time 20 secondsFrequency 48 kHzEquipment Power of …
Induction Shrink fit steel gear Class: Induction Shrink Fitting
Intro: Shrink fit steel gear Objective Heat the bore of a hardened spur steel gear to shrink fit onto a gear motor shaft. This is part of a chair for the disabled.Material Steel gear 2.5 h (63.5mm) OD, .75 h (19mm) ID x .625 h (16mm) thick, temperature indic…
Induction Shrink fitting carbide ring Class: Induction Shrink Fitting
Intro: Shrink fitting carbide ring Objective Shrink fitting a carbide ring into a steel valve seatMaterial Steel valve seat 6” (152.4mm) OD with 3” (76.2mm) ID hole & .75” (19mm) thick, carbide ringTemperature 500 F ( 260 C)Frequency 55 kHzEquipment •…
Induction Shrink fitting impeller blades to shaft Class: Induction Shrink Fitting
Intro: Shrink fitting impeller blades to shaft Objective Heat aluminum impeller blades to 200 F (93 C) and shrink fit onto a shaft.Material Aluminum impeller blades with a .28” (7.109mm) bore, aluminum shaftTemperature 200 F (93 C)Frequency 255 kHzEquipment…
Induction Shrink fitting pulley to insert bearing Class: Induction Shrink Fitting
Intro: Shrink fitting pulley to insert bearing Objective Heat aluminum pulley for insertion of an inner bearing for the automotive industryMaterial Aluminum pulley 2.3” (60mm) OD x 1.6” (40mm) ID x 1” (27mm) high and inner bearing 0.7” (17.8mm) high x 1.…
Induction Shrink fitting wrist pin into connecting rod Class: Induction Shrink Fitting
Intro: Shrink fitting wrist pin into connecting rod Objective Assemble connecting rods with a more accurate control of the heatMaterial Rod has an OD of .9125” (23.18mm), knuckle has an ID of .9125” (23.18mm) with an interference of .0001” (.0025mm). Knuc…
Induction Shrink Fit Camshaft Gear Class: Induction Shrink Fitting
Intro: Shrink Fit Camshaft Gear Objective: Heating a camshaft gear with a bore size of 1.630 to shrink fit over a steel shaft that has a diameter of 1.632. A temperature of 5000F is required for the gear to expand 0.002 in order to slip over the shaft. Produ…
Recommended
Air Cooled clamp coil (half-open coil) for preheating gas pipeline
U shape air cooled induction coil by UM-100C-HF for pipeline preheating
induction brazing diamond segment
induction melting for crystal growth
induction unassemble 2Ton guard ring of turbine
induction preheating D5000mm end ring for welding by 2 UM-DSP80A-HF at the same time
induction preheating D1219mm pipeline for welding by UM-DSB80AB-MF air cooled induction heater and i
induction preheating and heat treatment for 18Ton control valve of 600MW turbine